W/W -lead alloy 50-50 air cooled or W-Q is well known as a great alloy for consistent BHN increases for what ever use where increased BHN over pure lead (hardness) is desired . Hunting and getting less expansion at moderate yardage when trying to save the front shoulders being trashed by your favorite rifle. Also good for moderating the amount of slump in long profile boolits by again increasing BHN . I as others have a use for W/W cause it"s available and affordable ,and works pretty good as intended . I personally would not be shooting near as much with (store bought) alloys though acknowledged to be of more consistent quality , I make do/Ed